SRM 1-94 Compressive Properties of Oriented Fiber-Resin Composites
SRM 2-94 Compression After Impact Properties of Oriented Fiber-Resin Composites
SRM 3-94 Open-Hole Compression Properties of Oriented Fiber-Resin Composites
SRM 4-94 Tensile Properties of Oriented Fiber-Resin Composites
SRM 2R-94 Compression After Impact Properties of Oriented Fiber-Resin Composites
SRM 5-94 Open-Hole Tensile Properties of Fiber-Resin Composites
SRM 6-94 Compressive Properties of Oriented Cross-Plied Fiber-Resin Composites
SRM 7-94 In-Plane Shear Stress-Strain Properties of Oriented Fiber-Resin Composites
SRM 8-94 Short Beam Shear Strength of Oriented Fiber-Resin Composites
SRM 9-94 Tensile Properties of Oriented Cross-Plied Fiber-Resin Composit e
SRM 10R-94 Fiber Volume, Percent Resin Volume and Calculated Average Cured Ply Thickness of Plied Laminates
SRM 11R-94 Environmental Conditioning of Composite Test Laminates
SRM 18R-94 Glass Transition Temperature (Tg) Determination By DMA
SRM 21R-94 Fluid Resistance Evaluating of Composite Materials
SRM 22R-94 Determining the Resin Flow of Preimpregnated “B” Staged Material
SRM 23R-94 Determination of Resin Content and Fiber Areal Weight of Thermoset Prepreg with Destructive Techniques
SRM 25R-94 Onset Temperature and Peak Temperature for Composite Resin Systems Using Differential Scanning Calorimetry (DSC)
Sikorsky
SS9152/PP101 Determination of Glass Transition Temperature by DMA, Single Cantilever Method